Bevel Gear Heat Treatment

Carburising, Hardening, Induction Hardening and Nitriding for Bevel Gears: Hardness, Case Depth, Distortion Allowances and Finishing by Lapping or Grinding.

Heat Treatment Sets the Life of the Gear

Cutting gives the tooth its shape. Heat treatment gives it the hardness to carry load without pitting or wearing out. The route is written on the drawing or technical offer so that cutting allowances, finishing and inspection all follow from it.

Common Routes

  • Case hardening (carburising). The tooth surface is enriched with carbon, hardened and tempered. Surface hardness is commonly around 58 to 62 HRC over a tougher core. It is the standard route for spiral bevel and hypoid gears. A first estimate of effective case depth is often taken as roughly 0.15 to 0.2 times the module, then adjusted to the load.
  • Through hardening and tempering. The whole section is hardened to a chosen strength. It suits heavier sections and moderate surface loads.
  • Induction hardening. Only the tooth flanks or a selected zone are hardened. Useful for larger gears and for localised hardening.
  • Nitriding. A thin, very hard surface produced at a lower temperature, so distortion is small. It suits gears that are hard to finish after treatment.
  • Normalising and stress relieving. Used on forgings and after rough machining so that the gear stays stable during later cutting.

Distortion and Finishing Allowances

Hardening moves metal. Bevel gears are particularly sensitive because the teeth are curved and the section is uneven. The usual answer is to cut the teeth with a stock allowance, harden, and then finish by lapping or grinding so that tooth contact and backlash are brought back to the required values. The allowance is planned before cutting begins.

Lapped and Ground Sets

Lapping is done on the gear and pinion together, which is why a lapped spiral bevel pair is kept and used as a matched set. Ground gears are finished tooth by tooth and can be supplied individually, subject to the drawing.

Checks After Treatment

Depending on the order, we check surface hardness, case depth on a test piece, core hardness and the condition of the teeth after hardening, followed by contact pattern and backlash on the finished pair. Reports are given as agreed at quotation.

Frequently Asked Questions

What hardness do carburised spiral bevel gears reach?

Surface hardness is commonly around 58 to 62 HRC over a tougher core. The exact value and case depth are set by the drawing and the load.

Why do bevel gears distort in heat treatment?

Hardening moves metal, and the curved teeth and uneven section of a bevel gear make it more sensitive. A stock allowance is left on the teeth and removed by lapping or grinding after hardening.

Why are lapped bevel gears sold as a pair?

Lapping is done on the gear and pinion together, so the two members are matched. Replacing only one disturbs the tooth contact.

Which checks are done after heat treatment?

Surface and core hardness, case depth on a test piece, and then contact pattern and backlash on the finished pair, with reports as agreed at quotation.

Send Your Requirement

Share your drawing, sample details, quantity and delivery location. Our engineering team will review it and reply.